Evaluation of the Mechanical Strength of Concrete in Cylinders Dosed with Leachate at Different Concentrations
| dc.creator | Salvatierra, Sidney | es |
| dc.creator | Isa, Javier | es |
| dc.creator | Ríos, Roger | es |
| dc.creator | Fernández, Adriana | es |
| dc.creator | Salvatierra, Sidney | en |
| dc.creator | Isa, Javier | en |
| dc.creator | Ríos, Roger | en |
| dc.creator | Fernández, Adriana | en |
| dc.date | 2025-12-22 | |
| dc.date.accessioned | 2025-12-23T06:30:10Z | |
| dc.date.available | 2025-12-23T06:30:10Z | |
| dc.description | This study evaluates the impact of leachate on the mechanical strength of concrete by testing cylinders dosed with leachate concentrations at 100% water (0% leachate) in control quality, then at 50% and 100% leachate. One hundred and twenty-six cylindrical specimens (15 cm x 30 cm) were manufactured according to ASTM C31, distributed in three groups and evaluated at 7, 14, 28 days, and 3, 6, 9 and 12 months. The materials included the use of Portland cement IP30, siliceous and basaltic aggregates, and leachate from the Tiquipaya controlled dump (Cochabamba, Bolivia), characterized by a high organic load (COD: 7,520 mg/L), suspended solids content (28,140 mg/L) and an alkaline pH (9.9). The dosage used followed the ACI 211.1 method (water/cement ratio: 0.45). The results show that concrete with potable water maintained stable strength (221 kg/cm² at 12 months), while concrete with 50% leachate showed an initial reduction of 15-20%, recovering to 247 kg/cm² at 9 months. Concrete with 100% leachate achieved high initial strength, but suffered a 35% deterioration at 12 months (138 kg/cm²). These findings highlight the need to design concretes resistant to aggressive environments and improve leachate management in developing countries, proposing specialized cements and treatment systems to mitigate structural and environmental impacts. | en |
| dc.description | El presente estudio evalúa el impacto de los lixiviados en la resistencia mecánica del hormigón mediante ensayos en cilindros dosificados con concentraciones al 100% de agua (0% lixiviado) en calidad de control, luego al 50% y 100% de lixiviado. Se fabricaron 126 probetas cilíndricas (15 cm x 30 cm) según la ASTM C31, distribuidas en tres grupos y evaluadas a los 7, 14, 28 días, y 3, 6, 9 y 12 meses. Los materiales incluyeron el uso de cemento Portland IP30, agregados silíceos y basálticos, y lixiviados del botadero controlado de Tiquipaya (Cochabamba, Bolivia), caracterizados por una alta carga orgánica (DQO: 7,520 mg/L), contenido de sólidos suspendidos (28,140 mg/L) y un pH alcalino (9.9). La dosificación utilizada siguió el método ACI 211.1 (relación agua/cemento: 0.45). Los resultados muestran que el hormigón con agua potable mantiene una resistencia estable (221 kg/cm² a 12 meses), mientras que con 50% lixiviado presenta una reducción inicial del 15-20%, con recuperación a 247 kg/cm² a los 9 meses. El hormigón con 100% lixiviado alcanza alta resistencia inicial, pero sufre un deterioro del 35% a 12 meses (138 kg/cm²). Estos hallazgos resaltan la necesidad de diseñar hormigones resistentes a ambientes agresivos y mejorar la gestión de lixiviados en países en desarrollo, proponiendo cementos especializados y sistemas de tratamiento para mitigar impactos estructurales y ambientales. | es |
| dc.format | application/pdf | |
| dc.format | text/html | |
| dc.format | text/xml | |
| dc.format | application/epub+zip | |
| dc.identifier | https://revistas.intec.edu.do/index.php/cite/article/view/3592 | |
| dc.identifier | 10.22206/cite.2025.v8.3592 | |
| dc.identifier.uri | https://repositoriobiblioteca.intec.edu.do/handle/123456789/14975 | |
| dc.language | spa | |
| dc.publisher | Instituto Tecnológico de Santo Domingo (INTEC) | es |
| dc.relation | https://revistas.intec.edu.do/index.php/cite/article/view/3592/4327 | |
| dc.relation | https://revistas.intec.edu.do/index.php/cite/article/view/3592/4329 | |
| dc.relation | https://revistas.intec.edu.do/index.php/cite/article/view/3592/4330 | |
| dc.relation | https://revistas.intec.edu.do/index.php/cite/article/view/3592/4328 | |
| dc.rights | Derechos de autor 2025 Sidney Salvatierra, Javier Isa, Roger Ríos, Adriana Fernández | es |
| dc.rights | https://creativecommons.org/licenses/by-nc-sa/4.0/ | es |
| dc.source | Science, Engineering and Applications; Vol. 8 No. 1 (2025): Ciencia, Ingenierías y Aplicaciones; 85-110 | en |
| dc.source | Ciencia, Ingenierías y Aplicaciones; Vol. 8 Núm. 1 (2025): Ciencia, Ingenierías y Aplicaciones; 85-110 | es |
| dc.source | 2636-2171 | |
| dc.source | 2636-218X | |
| dc.source | 10.22206/cite.2025.v8i1 | |
| dc.subject | Hormigón | es |
| dc.subject | resistencia mecánica | es |
| dc.subject | dosificación | es |
| dc.subject | lixiviados | es |
| dc.subject | Concrete | en |
| dc.subject | mechanical resistance | en |
| dc.subject | dosaje | en |
| dc.subject | leachates | en |
| dc.title | Evaluation of the Mechanical Strength of Concrete in Cylinders Dosed with Leachate at Different Concentrations | en |
| dc.title | Evaluación de la resistencia mecánica del hormigón en cilindros dosificados con lixiviados en distintas concentraciones | es |
| dc.type | info:eu-repo/semantics/article | |
| dc.type | info:eu-repo/semantics/publishedVersion | |
| dc.type | Art. | es |